Sulfurous Acid Leaching of Kaolin for Preparing Alumina

The Bureau of Mines is conducting a program to evaluate technology for the recovery of alumina from domestic resources. Bauxite, the major alumina ore, is mainly imported. In recent years, bauxite-producing countries have formed an organization that attempts to control the supply and price of bauxite. The United States has only limited reserves of bauxite […]

Dry Washer

Dry washers have been used for many years in the Southwestern United States, where water is scarce, and especially in New Mexico where several million dollars in gold has been produced during the last century by dry washing. The Cerrillos, Golden, and Hillsboro districts are among those having produced gold by dry washing. In years […]

How to Stake a Mining Claim on Open Land

Instructions on staking claims and filing for patents can be obtained from the U.S. Bureau of Land Management. In addition to Federal regulations, individual States also have certain requirements pertaining to the location of claims on public lands. Information on these requirements is available from the State agency that deals with mining. Claims for mining […]

Gold Dredging Costs

In the section that immediately follows, specific cost data for dredge operations considered representative in the industry have been updated and listed. Following this is a section on general cost data that correlates operating costs to annual production according to bucket size. These costs cover dredge operations in the Western States. Cost of dredging in […]

Gold Dredge Sizing & Capacity

Determining Suitable Dredge Size: After the placer deposit is properly prospected the miner has a reasonable knowledge of the volume and grade of the placer together with information on its geometry, formation, and the distribution of values by size and location as well as information on bedrock topography, surface topography, water supply, and a host of […]

How to Determine the Value of a Placer Gold Deposit

The functioning and capacity of a dredging system must be keyed to the environmental and natural conditions of climate, water availability, location, and the physical and geologic characteristics of the deposit. The investigation of a placer deposit should be made by or be in charge of an experienced person or organization familiar with how these […]

Ferrous Scrap Steel

For the past decade, the Bureau of Mines has addressed the problem of using low-grade scrap, such as the ferrous fraction of municipal refuse, to produce steels of acceptable quality. The investigations are a part of the Bureau’s 65- year commitment to minimize the requirements for mineral commodities by devising new technologies for the recovery […]

Copper & Nickel Solvent Extraction

Nickel and copper were co-extracted from ammoniacal ammonium sulfate leach liquors (pH-9.5) with LIX 64N extractant in a laboratory-size mixer-settler continuous circuit. Three extraction stages resulted in >99-pct extraction of nickel, substantial copper extraction, and essentially no cobalt extraction from leach liquors. A crowd stage reduced the ammonia loading on the solvent by maximizing nickel […]

Sodium Silicate Uses & Applications

The practical application of common alkaline inorganic chemicals such as lime, soda ash, caustic, silicates and phosphates, in the beneficiation of minerals, is well known within the industry. These materials have been found to be useful throughout the flotation circuit. This paper discusses the chemistry of the soluble sodium silicates in relation to their use […]

Sludge Dewatering by Pressure Filtration

Pilot test results with 30% refuse slurry suggested the installation of two (2) Passavant Pressure Filters, Model 20 with 150 chambers each and a cake thickness of 40 mm. Each filter plate is 2m x 2m in size and the total cake capacity of each filter is 762 cu. feet. The sludge pumping requirements, per […]