Separating Gold from Silver by Electrolysis
This attractive method of separating gold from silver has made some headway, and will in many cases replace other methods of parting. The electrolyte used is a solution of silver nitrate, or it may be started with dilute nitric acid. The cathode consisting of thin silver plate and the anode of the silver-gold alloy usually in […]
Refining Gold with Sulphuric Acid

Pure silver is readily attacked by strong hot sulphuric acid of SG 1.815, or about 90 per cent, strength. The reaction which takes place may be represented as follows: 2Ag + 2H2 SO4 = Ag2 SO4 + 2H2O + SO2 Silver sulphate so produced is very soluble in the strong acid, when it is hot, as […]
How to Recover Silver from Nitrate Solutions
The usual method of recovering silver from these solutions is to precipitate the silver by means of common salt. From an ordinary alloy the only salts likely to be precipitated are mercurous chloride and lead chloride. The former would be present in traces only, and would be eliminated in subsequent operations. Lead is generally removed […]
Commercial Scale Gold Parting with Nitric Acid
The method of gold parting with nitric acid usually consists in: Granulating the alloy, which should he free from antimony, tin, or sulphides. Treating with dilute nitric acid, and decanting the solution. Boiling with strong nitric acid. Washing the parted gold free from alloy. Smelting the parted gold. Recovering the silver from solution. The granulating […]
Gold Parting using Nitric Acid

The process of parting gold with nitric acid is old, and probably dates from the discovery of nitric acid itself; it is one of the simplest parting processes, and does not require a costly plant or much manipulative skill. The main objection to it is the cost of the acid. The operation comprises the preparation […]
Miller Gold Refining Process by Chlorination

The term refining has been very often applied to the removal of base metals from the noble ones, or, in other words, separating the oxidizable from the non-oxidizable ones. When used in this sense it is generally applied to the term bullion, which is an alloy carrying gold and silver, the bullion being pure when […]
How to Refine Gold Bullion with Oxygen or Air

The how-to method of removing oxidisable metals by means of an oxidising agent has been practised for centuries. The operation has already been described in the cementation process with nitre, and the gaseous method of removing antimony from gold. The ordinary cupellation operations are also on the same lines. When oxidising fluxes are used, their action […]
How to Separate Silver & Gold by Cementation
Older processes explaining how to go about separating silver from gold by cementation were carried on practically in two ways, the first by heating gold for a long time with a mixture which evolved nitric acid on heating, and an absorbent into which any fusible salts ran; the mixture in the second method contained common salt […]
Common Uranium Minerals Classified by Colors

Name Chemical Composition %U3O8 Color Luster Hardness Specific Gravity SG Characteristics & Occurrence Pitchblende Uranium oxide 50-80 Black (Grayish, Greenish) Pitch like Earthy, Dull or Glassy 5-6 6-9 In Veins; often with Sulphides of Cobalt, Nickel,Silver, Bismuth or Yellow Secondary Uranium Minerals. Never Brownish or Reddish. Uraninite Uranium oxide 65-85 Black (Grayish, Greenish, Brownish) Pitch like […]
Sulphur Refining of Gold

Refining with Sulphur A more speedy method of removing iron, copper, lead and base metals from bullion is to add sulphur to the molten metals. Although gold sulphides may be readily formed in the wet way, they are decomposed into gold and sulphur by merely heating them to a temperature below 300 deg. C. If […]