Assess Permeability Enhancement In Situ Mining

blasting-test polyaxial confinement cell

In situ recovery of minerals has great potential as a mining technology to mine deposits that might otherwise be overlooked by conventional techniques. Some hard-rock deposits, however, will not have adequate permeability to permit successful in situ mining and will require permeability enhancement of the rock deposit prior to leaching. The leaching process in this […]

Aerophine 3418A Collector for Precious Metals Flotation

flotation polymetallic ore data evaluation

The origins of AEROPHINE 3418A promoter date back to the 1960’s, when it was established that sulfide mineral collectors based on phosphine chemistry demonstrated efficacy. This new collector chemistry was found to provide flotation performance differing significantly from those of more traditional thiol collector chemistries such as xanthates, dithiophosphates, mercaptobenzothiazoles, thionocarbamates and those with xanthogen […]

Blast Optimization and Ore Fragmentation Modeling

fragmentation-blast-design

Blasting plays a key role in all facets of operations. Obviously, drilling and blasting costs are determined by blast design, but the downstream costs that are closely related to blasting results are often treated as separate functions: loading, hauling, cleanup, and crushing and grinding are all heavily influenced. Diggability and bucket fill factor are a […]

Mine Ventilation Recirculation Systems

recirculation ventilation schematics

In many deep mines, the design of a ventilation system to satisfy the airflow requirements might be difficult to implement and expensive to maintain. The problem may even be more serious when the mine workings are dispersed and located a considerable distance from the surface connections. This problem can be alleviated by including a controlled […]

Extract Tantalum & Niobium from Pegmatites

wyoming-pegmatites low-grade samples

The Bureau of Mines’ Intermountain Field Operations Center, Denver, CO; and the Bureau’s Salt Lake City Research Center, Salt Lake City, UT, jointly studied domestic sources of tantalum and niobium as part of the Bureau’s program to reduce national dependency on imported minerals and metals that have key uses in industry and defense. Presently the […]

Germanium Extraction from Zinc Hydrometallurgy

germanium-extraction zinc processing flowsheet

Germanium is an important strategic metal used in fiber optics, infrared detectors, and semiconductor devices including transistors, diodes, and rectifiers. Substitution for germanium cannot be made without substantial loss in performance in most cases. Germanium is generally not concentrated naturally, although trace amounts are found in many minerals. Germanium is produced almost exclusively from waste […]

Apatite Leaching using H2SO4 & Methanol

apatite-particles scanning electron photomicrograph

Current practice for the production of wet-process phosphoric acid (H3PO4) involves leaching beneficiated phosphate rock with aqueous H2SO4. Typical processing involves mining the ore, also called matrix, using a dragline, then forming a water-based slurry to facilitate pumping the ore to a beneficiation plant. Phosphate values contained in the minus 150-mesh fraction of the ore […]

Effect of Chromium on Wet Grinding Performance

wet grinding bulk microstructures

Because of higher efficiency, wet grinding is more widely used than dry grinding, but leads to an increased consumption of grinding media due to corrosion in some ores. In dry grinding, the wear rate of high chromium cast irons is frequently ten times lower than cast or forged steel with a cost ratio of 2-3 […]

Heap-Leaching Pad Volume Calculations

heap-leaching wharf resources

The estimating of volumes is a routine practice in an open pit-heap leaching operation. Until recently, the conventional cross-section manual method has been used at Wharf Resources’ South Dakota operation for the estimate of material mined from the pits, crushed ore delivered to the heaps, unload spent ore, ore and topsoil stockpiles, waste dumps and […]

Reprocessing Gold Tailings by Gravity Methods

auriferous-gravity-tailings influence of grinding time

Tailings originating from the gravity concentration of a gold ore containing about 14 g/t Au have been treated by various beneficiation methods. These tailings have been screened on the 147 and 74 micron sieves and the two coarsest fractions have been separated on shaking tables with unsatisfactory results, but the concentrates have been examined in […]