IsaMill
Look inside an IsaMill and have a look at an installed IsaMill grinding unit. IsaMill Signature Plot
Ultrafine Grinding Test Report AKA IsaMill Signature Plot

Here is an energy plot AKA an IsaMill Signature Plot AKA a Ultrafine Grinding Test Report. This test is performed using a Netzsch Grinding lab mill. I also include links to great articles about this powerful ultra-fine grinding technology. 1) IsaMill- 1:1 Direct Scaleup from Ultrafine to Coarse Grinding 2) The Benefits of IsaMill Testing 3) Industry/Research Papers from […]
How to Interpret Particle Size Distribution Data

For a great presentation on How to Interpret Particle Size Distribution Data D50 D80 D90 and D10 you need to see https://www.brainshark.com/malvern/particlesize_mining_mineral/z8azT04z0z0?v=3 by Malvern.
List Gold Producers

Let me list for you several/most gold producers as of 2013
Optimum Froth Bed Depth Levels

When the pulp levels on all cells appears high (shallow froth bed thicknesses or depth). This causes unstable froth which constantly produces a low density “run-away” or wet, watery un-drained rougher concentrate rich in mechanically floated (entrained) “other materials” and containing most of the frother (added to flotation feed) itself. ** Operating at shallow froth […]
Compare Hydroxamate AM2 Rinkalore CTC3 Oxide Collectors
In this series of tests aimed to Compare Hydroxamate Collectors namely: AM2 Rinkalore and CTC3 we now conclude. All data indicate the CTC3 is a more selective reagent. In all tests, metallurgy was improved. Nowhere were the results produced by CTC3 inferior to AM2. Although AM2’s Lab Recoveries can look “attractive”, the AM2 reagent shows problematic […]
Oxide Flotation Collector | Collector for Copper Oxide Ore

In this flotation tests and evaluation for the best collector for copper oxide “ore” 911Metallurgy continues with material that’s 60% Oxide copper. Sample C: 1.7% Copper about 60% Oxide Cu Rougher Tests: Both reagents appear to behave similarly as the “blue dots” are seemingly a continuation of the trend started by “red dots”. Oxflo and Axis […]
Flotation by Hydroxamate: OXFLO- CTC vs AXISHOUSE-AM2

The order of Hydroxamate flotation testing was first OXFLO for 3 days, then AXISHOUSE’s tests were performed 3 weeks later for 7 days. The results of each “Ore Type” or Samples tested by OXFLO (OxF) and AXISHOUSE (AH or Axis) is graphically displayed and evaluated in this report. Prior to testing their chemicals, each “Ore […]
Hydroxamate for Copper Oxide Flotation

Here is a comparison of two Hydroxamate Collectors used for the flotation of Oxide copper, namely CTC3 from OXFLO and AM2 (AKA Rinkalore) from AXISHOUSE. This report contains a comparison of the scoping test-work done by both suppliers to determine which one is the best Oxide Collector . Test Summary #1 Flotation by Hydroxamate: OXFLO’ […]
OXFLOAT CTC3
The earlier versions of OXFLOAT CTC3 had been in production since 1972 and currently Oxflo’s manufacturing partner supplies 700 mt of this product to their local market annually. They have a further manufacturing capacity of 800 mt, taking them to a total of 1500 mt per year. Currently OXFLOAT CTC3 has displaced AM2 at one […]