Estimated/Approximate Rubber Liner Wear Life/Rate Cost

In a Ball Mill (particularly) the wear rate or wear life of Rubber depends much on the Ball Size/Diameter used in that mill. The grinding media size which itself is much of a function of the ore/material P80 feed size into that mill. The other primary and addition factor contributing to a mill rubber liner […]
Compare Mechanical Flotation Cell & Column Cell
Flotation Column Cell Carrying Capacity & Scale-Up

Flotation Column Cells can only ‘carry’ or recovery so much froth/concentrate for any given diameter. Unlike a mechanical cell on which you can just turn-on more air to recover more metal, column cells with not respond that way. A column cell can only carry so much froth to the concentrate launder. Their concentrate production is […]
Gravity Gold Recovery and Gold Flotation Recovery Process
Gold Extraction from eScrap CPU Computer Chips

Electric gold melting furnace Portable Torch Cutting Welding Vacuum Filter Kit with Hand Pump Magnetic Stirrer pH and Thermometer Gas Mask Chemical Protective Clothing Glove Chemical Boots Chemical goggles Digital Scale 0.001 g Hot Plate Alcohol Lamp Spoon Glass Stir Sticks Distilled Water Bottles Glass Baster Filtering Flask Stainless Steel Beaker Polypropylene Buchner Funnel Filter […]
Black Sands Processing & Content Assaying

It appears none of the gold prospectors spend nor time or money on assaying their black sands for gold value determination. Instead, they use a rare earth magnet to tells them what is in there and see that most of the gold is magnetite with sometimes hematite. What little remains goes under the microscope where […]
How a Rod Mill Works
D12 Laboratory Flotation Machine Drawings & Dimensions

D12 Laboratory Flotation Machine Drawings & Dimensions In case you need the specific sizes: depth, height, weight, width of you lab float cell.
Hydrocyclone Rubber Liners

We sell Rubber Liners for Hydrocyclone: You can buy parts like the main body liner, lower cone and Apex or Vortex. Long lasting, good wear and better price VS life relationship than a Linatex types Brand.
Copper Lead Concentrate Separation

The ways to obtain successful Separation of Copper and Lead into individual Concentrates, several process approaches can be examined; bulk copper-lead flotation with a reverse flotation stage depressing copper, the same bulk flotation with a reverse flotation to depress lead and a sequential copper-lead-zinc flotation circuit as well as a simple cleaning of the bulk Cu/Pb concentrate by Pb […]