Concentrator Operator – What does a Mill Man Do

The manual is aimed at laying out the basic tasks a good mill operator needs to perform and master on the path to becoming a good concentrator operator. This guide will provide a source of reference material for the operator and an instructional text containing material giving the operator a basic understanding of the purpose […]
Gold Chlorination Process by Miller

Miller’s Gold Chlorination process was introduced by F.B. Miller. The refining process employs chlorine gas, which passed into molten gold covered with a layer of borax and silica, and reacts with most of metals present in the molten charge. Platinum group metals do not react. Basically, gold is slightly attacked in the first moments and […]
Pruebas de ciclo cerrado y su procedimiento

Una prueba de flotación de ciclo cerrado (locked cycle test en inglés) es usualmente efectuada al final de un programa de pruebas de flotación de laboratorio, y tiene como objetivo principal confirmar las mejores condiciones de flotación obtenidas en la etapa de pruebas abiertas. Para lo cual se busca evaluar la dosificación de los reactivos […]
Mesa de Concentración Gravimétrica – Uso y Funcionamiento

La mesa de concentración gravimétrica suele usarse a escala industrial para limpiar concentrados gravimétricos impuros, y a nivel laboratorio para evaluar la presencia de minerales pesados. El caso más común de uso es el tratamiento de metales preciosos, y de minerales de estaño como la casiterita. Es importante indicar que la concentración gravimétrica ha sido […]
Indice de Trabajo de Bond y su Procedimiento

El índice de trabajo de Bond se ha usado por muchos años para indicar el consumo de energía de un molino de bolas para obtener un tamaño de partícula deseado, usualmente expresada como el pasante bajo una malla especifica como la 150 o la 200.el valor del índice de trabajo de trabajo es una característica […]
Conceptos Básicos de Flotación de Minerales

El proceso de flotación de minerales está basado en procesos fisicoquímicos que ayudan a explicar la afinidad de algunas partículas al aire (esta característica es llamada hidrofobicidad), y también de la afinidad de otras partículas minerales por el agua (esta característica es llamada hidrofilicidad). El objetivo del proceso es tratar de obtener un producto comercial […]
Mineralogy Point Count Procedure

The point count procedure was to select an appropriate magnification for the micro mount ranging between 100 – 1000 times normal, and then setting a 10×10 square graticule randomly on the field. Mineral grains which were intersected by the graticule cross hairs, were identified and recorded and entered directly into the computer using a […]
Types of Anionic Collectors of Sulphides

Collectors for sulphide minerals : Anionic collectors are most commonly used for sulphide minerals. By reference to the table (below) it will be note that they are all structurally similar, each having a single sulphur atom double bonded to either a carbon or phrosphorus atom, hence all of the sulphide minerals can be floated with […]
Cassiterite Flotation – Tin Oxide

The nominal size range for cassiterite flotation is between 2 and 100 microns. The top size is variable depending upon the liberation of the cassiterite particles. Cassiterite grains coarser than 100 microns are difficult to float whilst grains finer than 2 microns give selectivity problems. Hence the feed for cassiterite flotation should be reduced to […]
Froth Flotation of Tungsten Ore

Scheelite (CaWO4) and Wolframite ((Fe,Mn)WO4) are the principal minerals of tungsten, but other important minerals include ferberite (FeWO4) and huebnerite (MnWO4) will also respond to froth flotation. The high specific gravity of these minerals makes many of these ores amenable to gravity concentration methods, however, the fine dissemination of mineral in gangue for some ores […]