Ball Mill Gear
Two general classifications of gearing are used for ball Mill drives. These are the spur gear and the helical gear. Helical gearing may be either of the single helical or double helical (Herringbone) design. SPUR GEARS These are generally furnished on the smaller diameter mills using V-belt drives or reducer drives. Spur gears and pinions … Read more