carbonate absorption pilot plant
Hydrometallurgy

Hot Potassium Carbonate Absorption

Hot carbonate purification will remove hydrogen sulfide from gas mixtures of low or high concentration of this component. The presence of some carbon dioxide in

Read More »
blast furnace experimental-scale rotating disk pelletizer
Smelting - Melting - Refining

Smelting Unfired Iron Ore Pellets

Fines and concentrates must be consolidated or agglomerated into larger masses before they can be smelted in a commercial blast furnace. Such agglomeration is usually

Read More »
leaching of uranium mill flowsheet
Hydrometallurgy

Pressure Leaching of Uranium

Early studies in the carbonate leaching of uranium ores led to the investigation of pressure leaching as a method to enhance the dissolution of the

Read More »
bastnasite flowsheet
Hydrometallurgy

Rare Earth Oxide Bastnasite

A bastnasite concentrate, containing about 60 percent rare earth oxides, was sulfated with concentrated sulfuric acid to eliminate the carbon dioxide, fluorine, and silica. Calcination

Read More »