Aluminum Chloride Hexahydrate from Kaolinitic Clay
Table of ContentsMaterials and ProceduresResults and DiscussionFlowsheetEconomics There has been considerable interest in developing methods to economically produce cell-grade alumina from nonbauxitic materials. In the