Heap Leach Feed Preparation

Some gold and silver ores are difficult to successfully heap leach because of the high percentage of clay, and/or fines which are intrinsic in the

Read More »

Heap Leaching at Altitude

It is feasible to conduct cyanide heap leaching at high altitudes as has been demonstrated by a number of pilot and commercial operations in the

Read More »

Heap Leaching with Sea Water

There are locations on the west coast of South America, in Australia, and in the California internal desert where fresh water is practically unavailable. It

Read More »
Various

Bioleaching Carbonaceous Gold Ores

The previous tests demonstrated the use of facultative and extreme thermophiles for refractory sulfide gold ores and flotation concentrates. The following tests were conducted on

Read More »

Flotation Training

https://www.911metallurgist.com/flotation-recovery-cumulative-grade-recovery-curve https://www.911metallurgist.com/mineralogy-flotation-floatability-selectivity https://www.911metallurgist.com/flotation-mass-water-recovery-mineralogy Laboratory Flotation Testing Services

Read More »
Various

Cyclic Voltammetry

A few representative cycles from the first 20 oxidation/reduction cycles for a pyrite electrode in 0.1 M sodium borate are presented in Figure 3. The

Read More »
Various

Pyrite Buffer in Soil

The Gunnison, Colorado, tailings provide an example of the chemical reactions across the interface with soils rich in pyrite but low in calcite. In this

Read More »

Laws of Gravity Gold

Ten Laws of Gravity Gold Recovery DO DON’T Try to Evaluate the Economic Impact of Gravity Recovery Get a Statistically Significant Sample of the Ore

Read More »