Paste Backfill Fundamentals
Paste is a high density mixture of water and fine solid particles with a relatively low water content (10-25%) such that the mixture has a
Paste is a high density mixture of water and fine solid particles with a relatively low water content (10-25%) such that the mixture has a
Selective flocculation was used to produce superclean zinc concentrate with minimized silica contamination. Research was carried out on a flotation concentrate from the Jersey Miniere
The unique application of a large walking dragline in the mountains of southern West Virginia was developed and implemented by Hobet Mining, Inc. Hobet is
Mining has never been a major source of income for Puerto Rico. The Spaniards mined gold placer deposits during 1509-1579, and extracted an estimated 1,200,000
A series of tests were undertaken for the Aurora Partnership-Aurora Project to solve inter-laboratory variations in the analyses of blast hole cuttings. Initial concern was
Treater Dust is the name given to the material that is collected in electrostatic precipitators used for off-gas cleaning of elemental phosphorus furnaces. Elemental phosphorus
Typical dragline rigging includes several sets of ropes: hoist ropes, drag ropes, dump ropes and boom suspension ropes. The drag and hoist ropes contribute most
Pyrite oxidation has been studied extensively in relation to its role in sulfide mineral flotation. Although pyrite usually lacks economic value in polymetallic ores, it
Serpentinite minerals are available in large quantities from asbestos mining activity. The granular or fibrous serpentite, at temperatures greater than 700°C, will recrystalize into olivine,
An acid mine drainage sludge sample containing 3.6% Mn, 0.18% Ni, 0.15% Co and 0.39 % Zn was obtained from the central part of West