Pressure Oxidation Leaching Process

Batch Autoclave Laboratory Procedures: The vessel used for the laboratory pressure oxidation process was a two-liter Parr titanium autoclave with dual impellers. It was heated and

Read More »

Infill Drilling Program Design

An exploration process is normally consisted of four major phases: regional reconnaissance, detailed mapping, sparse drilling, and infill drilling. Regional reconnaissance focuses on promising areas

Read More »

Magnetic Separation of Clay

Conventional Magnetic Separator: An Eriez conventional high gradient magnetic separator (HGMS), model EL 20-4, with a 0.058 m canister diameter and a total volume of 1030

Read More »