In this module, I’ll take you through the key aspects related to underground mining activities. In this module, we will look at economic considerations in

In this module, I’ll take you through the key aspects related to underground mining activities. In this module, we will look at economic considerations in

Welcome back to the surface mining model. In the previous topic, we learned about different types of surface mining operations, about equipment, about different methods

In the previous topic, we saw that blasting is the mining operation used to break the rock mass in order to facilitate the removal of

The previous topic has established that surface mining operations include several main activities that include the ore extraction or mine of the material, the overburden
In the concept of mining a deposit, mining operations should be planned and organized in order to maximize the productivity. Slope stability issues directly affect

First of all let’s define what we mean with surface mining. Surface mining means the extraction of mineral deposits or coal reserves or stones of
Rock mass failure does not always involves discontinuities. There are cases, especially for excavations, like the tunnel you see on this photo where the stress

In previous topics, we have seen that discontinuities constitutes as a weakness in the rock mass. In fact, failure of a slope, for example, is

In previous topics, we’ve discussed strengths of materials because failure typically occurs when stresses exceed the strengths, it is important to know the stress distribution

For most rock engineering projects, it is required to characterise not only the intact rock, but also the rock mass as a whole, and this