Copper Lead Zinc Metallurgy
Monthly composites of mill feed, copper concentrate, lead concentrate, zinc concentrate and final tailing were sent for detailed mineralogical/metallurgical analysis. These samples were analyzed and also

Monthly composites of mill feed, copper concentrate, lead concentrate, zinc concentrate and final tailing were sent for detailed mineralogical/metallurgical analysis. These samples were analyzed and also

In a certain case study of “high” Arsenic in Copper Concentrate (almost 0.5% As) produced by flotation, and where the Cu Conc is mostly chalcopyrite and

Just an example of strength at which flotation reagents can be mixed at in a Concentrator:

What is x-ray fluorescence and why is XRF sample preparation is important for correct XRF analysis. This is a little introduction to some of our instruments;

Here I will be focusing on a chemical surface technique called X-ray Fluorescence Spectroscopy, this method is of importance because it is widely used for
A ABC Assay Based Controls are changes made to regulatory set-points that are biased on the level or changes in the level of the

Here are rough instructions to perform a sequential flotation locked cycle test procedure to assess the overall metallurgy of an ore sample expected to produce only 1

In a lab float test, you adjust to agitator’s RPM based on the volume of the tank you’re working with. Here are suggestions. Rougher Cell: