Tungsten
Flotation

Froth Flotation of Tungsten Ore

Scheelite (CaWO4) and Wolframite ((Fe,Mn)WO4) are the principal minerals of tungsten, but other important minerals include ferberite (FeWO4) and huebnerite (MnWO4) will also respond to

Read More »
Laboratory Flotation Testing
Flotation

Laboratory Flotation Testing

Batch Laboratory Flotation Testing starts from the 3 fundamental types of flotation processes or methods which can be classed as either: Bulk flotation Differential flotation

Read More »
Rod Mill Charger Loading Machine
Grinding

How to Charge Rods into a Rod Mill

Rods are loaded or charged into a Rod Mill using a mechanised charger.  The rod charger with extendable boom moves rods safely inside the trommel/trunnion before charging

Read More »
Column Leach Test
Cyanide Leaching

Column Leaching Procedure

1) For better Column Leaching, Agglomerate ore if required. The procedure is to cure for recommended time period. During this time the ore should be kept damp via

Read More »
Small Home Hobby Cyanidation Bottle Roller
Concentrator Manuals/Procedures

Cyanide Gold Extraction Process

Here is a method on how to conduct a cyanidation bottle roll test AKA Cyanide Gold Extraction Process: Riffle out 400 grams of the ore. Grind