Impact Work Index Procedure
Crushing & Screening

Impact Work Index Procedure

This is or was used by Sandvik to acquire the Impact (AKA Crushing) Work Index for sizing crushers.  Use this in complement to the Bond Crushing

Read More »
BWi
Concentrator Manuals/Procedures

Bond Grindability Test Procedure

The Bond Ball Mill Grindability test is designed to give a measure of the grinding characteristics of a material by finding the amount of size reduction

Read More »
KNELSON CONCENTRATE OF INTRUSION
Geology

Fine Gravity Gold

Here are images of gold ores rich in sulfides including arsenopyrite.   Some of the ore types in these photos: https://en.wikipedia.org/wiki/Breccia https://en.wikipedia.org/wiki/Hornfels https://www.merriam-webster.com/dictionary/intrusion https://en.wikipedia.org/wiki/Limestone https://en.wikipedia.org/wiki/Volcanogenic_massive_sulfide_ore_deposit

Read More »

Disclaimer

Nothing contained in the calculators, equations or other information on this website constitutes advice. Access to the calculators, equations and other information is donated for

Read More »
Mineral Processing Laboratory
Equipment

Mineral Processing Laboratories

Finding a good and the right mineral processing laboratory and have your testing filled properly is important. Most metallurgical laboratories now are actually specialized. They will

Read More »
Sampling a Conveyor Belt
Feeders and Conveyors

Sampling a Conveyor Belt

To sample a FINE free-falling stream (Sampling a Conveyor Belt with a cross-belt cutter) as depicted, a sampling cup shall be used with the minimum

Read More »