Pb Oxide Floatability & Selectivity VS Sulphidizer Usage
The use of a sulphidizer is common in oxide flotation recovery. Na2S (Sodium Sulfide) can help “activate” oxide minerals behave as sulfides. The tests performed
The use of a sulphidizer is common in oxide flotation recovery. Na2S (Sodium Sulfide) can help “activate” oxide minerals behave as sulfides. The tests performed

It is clear the Pre-Float stage creates much looses in Cu, Au and Ag. Mineralogy work on this stream would help understand why the metals

Continuing with the evaluation of copper oxide flotation using hydroxamate we now evaluate a rock that’s 41% copper oxide with some lead oxide included. Sample

What is flotation mass pull and why does it matter so much? If we consider the total Plant Feed of 2800 TPD as 100% of

When are steel liners better than rubber/poly-met liners in a SAG mill or Ball Mill? Let’s compare! Rubber Liners are better for abrasion grinding ie:

https://www.911metallurgist.com/milling-calculations-formulas

An example of how you can calculate the slurry flow/volume of a given SG, %Solids and Tonnage. EXAMPLE: 3,400 tons of dry solids is processed

Ore specific gravity Pulp Density Relations

Here is the formula for specific gravity of a slurry, S is: S = specific gravity of slurry Si= specific gravity of liquid phase Ss= specific