Chile’s port strike affects copper exports

A two-week strike at the Angamos port is severely affecting Chile’s copper exports and the main companies operating in the country. Almost $130 million worth of Codelco’s December income has been sliced due to the tie-up, now joined by six other Chilean terminals. Workers at the seaports of Iquique, Antofagasta and San Antonio, for instance, stopped […]
Chile uses desalinated water in mining processes

The use of desalinated water in mining processes might become a mandatory action in Chile, after the submission of a new draft bill. The action was carried by the country’s lower house members, who want to fight the decreasing supply of the vital element, as well as provide a solution to the industry mounting power needs. […]
Sun might be the answer to Chile’s energy shortage in the mining industry

The Coquimbo region, in the arid region of northern Chile, just opened the first solar plant for the mining sector in the area. The goal is to end all power supply issues that have been affecting the work in a region that is the world’s number one in copper production. The country’s Energy minister, Jorge Bunster, […]