Some type of Magnetic Separator¬†is always advisable and should be a standard piece of equipment in every mill. When one (Suspended Type) Magnet is located just ahead of the primary jaw crusher, and another is placed before the intermediate crusher, all danger of damage to the crushers from tramp iron is eliminated. The tramp iron … Read more

Electromagnetic Separation

Starting with a mixture of any of the above minerals it may be determined whether or not they can be separated by¬†high tension, magnetic, or gravity methods and whether any one, or a combination of “Electromagnetic Separation” methods is required. If the minerals appear in different columns they may be separated by high tension and/or … Read more