Disseminated Polymetallic Ore Deposits – Mineralogy

Disseminated Polymetallic Ore Deposits - Mineralogy - 911Metallurgist

You do not know what Disseminated Polymetallic Ore Deposits or Complex Mineralogy until you have seen a QEMSCAN like this: With simple main observations as crazy as these below. ***The proportion of each mineral liberated at a 56µm grind P80 was: Chalcopyrite — 36% liberated Galena — 12% liberated Sphalerite — 45% liberated Pyrite — 85% liberated […]