Flotation Residue Disposal

Distributor

There are many methods of handling sand and slime from metallurgical operations, but in this article the draining and conveying of waste products from flotation processes will be specially dealt with, the methods given being those in use at the leading flotation plants in Australia. DRAINING AND DEWATERING It is generally advisable to thoroughly dewater […]