Fluorspar Extraction Processing Flowsheet

Fluorspar or Fluorite; CaF2. — Color, white, yellow, green, red, blue, deep purple, sometimes brown; powder, white; luster, glassy; H = 4; G = 3.01 to 3.25; crystals, in cubic system, mostly cubes; cleavage, perfect, cleavage pieces tending to show equilateral triangles which are also often to be seen outlined by cracks and edges; composition, […]