A Gold Shaking Table are basically low-capacity machines used as last step in the gold upgrading process. The shaking table is a thin film, shear flow process equipment, that separates particle grains of its feed material based on the differences in their specific gravity, density, size and shape. Mineral rich particles, from light to heavy and fine to coarse will […]