Slurry Stream Sample Cutter Dimensions for Grinding Circuit Survey

A good grinding circuit survey (and flotation circuit sampling) is only as good as the sample cutter used for each slurry stream. Correct sampler volume and opening size insures your sample is representative of the concentrator stream you are testing. Here is a good suggested design with opening dimensions. You need to add the handle […]