Open Stope Mining Method
Speaking generally, in the Open Stope Mining Method, the jasper hanging walls of most of the deposits in the Iron River district dip at a steep angle and are exceedingly strong, standing without caving, even after mining has been continued for years and after large excavations have been made. The ore is fairly hard and … Read more