Molybdenum Ore Processing by Flotation

This molybdenum flotationĀ circuit, based on 250-500 tons per 24 hours is designed for low-grade molybdenum ore having high-grade streaks and with pyrite-quartz gangue. It is also basically sound for many other friable sulphide ores, such as antimony, silver and even some lead ores. The basic ideas stressed in this moly flotation flowsheet are the importance […]