Millerite Serapation from Pentlandite and Chalcopyrite

While there are over 45 different nickel minerals, only a few of them are of economic importance to the minerals industry. The principal nickel mineral in nickel sulphide ores is pentlandite ((Ni,Fe)8S9) while the less common nickel sulphides include millerite (NiS). violarite (Ni2FeS4), polydymite (Ni3S4), siegenitc {(Co,Ni)3S4), and heazlewoodite (Ni3S2). As well, often present are […]