Oxide Flotation Collector | Collector for Copper Oxide Ore

Oxide Flotation

In this flotation tests and evaluation for the best collector for copper oxide “ore” 911Metallurgy continues with material that’s 60% Oxide copper. Sample C: 1.7% Copper about 60% Oxide Cu  Rougher Tests: Both reagents appear to behave similarly as the “blue dots” are seemingly a continuation of the trend started by “red dots”. Oxflo and Axis […]

Flotation by Hydroxamate: OXFLO- CTC vs AXISHOUSE-AM2

Hydroxamate CTC3 vs AM2 Rinkalore

The order of Hydroxamate flotation testing was first OXFLO for 3 days, then AXISHOUSE’s tests were performed 3 weeks later for 7 days. The results of each “Ore Type” or Samples tested by OXFLO (OxF) and AXISHOUSE (AH or Axis) is graphically displayed and evaluated in this report.  Prior to testing their chemicals, each “Ore […]