Silver Lead Zinc Ore Processing Method using Flotation

Silver Lead Zinc Ore Processing Method using Flotation - 911Metallurgist

Sulphide ore of lead and zinc containing considerable silver was submitted for testing with the purpose of determining a flowsheet for the production of separate lead and zinc concentrates for marketing at their respective smelters. It is necessary to recover as much silver as possible in the lead concentrate as a higher return for this […]

Flotation Circuit Startup and Shutdown Procedure

flotation_machine

In preparation for this EXAMPLE Startup, the following items must be checked before the associated conditioning and flotation equipment and circuit is started. Ensure that all applicable reagent systems are operational, and that the conditioning tank agitators, flotation feed pumps, flotation mechanisms, flotation blower, and the rougher concentrate, cleaner tails, and argentite leach feed pumps are operational. The samplers […]

Silver Mineral Argentite Flotation Circuit

flotation_machine

Solid residue from the second filtration stage is repulped with reclaim water to 35% solids, and is pumped to our EXAMPLE Conditioning and Argentite Flotation Circuit which is a process for the recovery of this Silver Mineral. A large portion of the silver in the ore will not have been leached in the initial grinding and […]