The Sink and Float separation process is part of what is also known as a Heavy Media Separation Process (HMS) and are commercial adaptations of the common laboratory procedure used for separating a mixture of two products having differentials in specific gravity by immersing the sample in a heavy liquid having a gravity intermediate to those of … Read more

Dense-Heavy Medium Separation HMS / DMS Process

DMS Dense medium separation

HMS and DMS are acronyms for Heavy (Dense) Medium Separation and is applied to the process of pre-concentration of minerals – mainly the production of a high weight, low assay product, which may be rejected as waste. In principle it is the simplest of all gravity processes and is a standard laboratory method for separating minerals … Read more