Leach Gold using Hyposulphite Of Sodium AKA Thiosulfate Gold Extraction

  The fact that gold will dissolve in sodium hyposulphite solutions is known from the lixiviation of silver and gold ores.┬áThe gold will dissolve only in small quantities. According to researchers, if gold leaf is treated for a time with sodium hyposulphite solutions of varying strengths,’ solution takes place in every instance, the deviation in … Read more