Extracting Tungsten from Wolframite Gold Ore

The present great demand for tungsten due to world conditions has resulted in an increase of tungsten ore dressing problems for our metallurgists. The flowsheet study shown here was recently developed for treatment of a very complex tungsten-gold ore. The flowsheet study previously shown for tungsten was devised for a simple tungsten ore free of […]