Merrill-Crowe Zinc Precipitation Startup and Shutdown

The Operation of a Merrill-Crowe Zinc Precipitation circuit requires for Preparation for its Startup that the following items be checked before the equipment in the Merrill-Crowe Zinc Precipitation Circuit is started. Note the levels in the pregnant solution, clarified solution and barren solution tanks. The pregnant and barren solution tanks should be approximately half full. If the pregnant solution tank is full […]
Merrill-Crowe Zinc Precipitation Circuit Operation

In the Merrill-Crowe Zinc Precipitation, the pregnant solution tank collects the gold and silver bearing solution recovered from other circuits of the plant: thickener overflow; primary and secondary filtration? and the Argentite circuits. Normally these solutions contain very little solids content (15-100 ppm), however, even this small amount of solids is sufficient to inhibit efficient […]