Lead Zinc Sulfide Separation by Sequential Flotation

Galena

In the majority of the zinc operations, sphalerite (ZnS) is associated with galena and often sulfides of iron and copper. It is therefore essential to arrange the flowsheet not only for recovery of the valuable minerals, but also to selectively separate them into products acceptable to the smelters for ultimate conversion into metal. The flowsheet outlined […]

How to Process Oxidized Lead-Zinc Ore by Flotation

How to Process Oxidized Lead-Zinc Ore by Flotation - 911Metallurgist

The problem of treating oxidized lead-zinc ores for the production of high-grade lead zinc concentrates is a complex problem due to the nature of the ores and to the soft sliming characteristics of the lead and zinc minerals. The ore for treatment is a lead-zinc carbonate ore in a mixed siliceous-lime carbonate gangue. The association of […]

Galena – Sphalerite Flotation & Separation Method

Galena - Sphalerite Flotation & Separation Method - 911Metallurgist

The problem of treating oxidized lead-zinc ores for the production of high-grade lead zinc flotation concentrates is a complex problem due to the nature of the ores and to the soft sliming characteristics of the lead and zinc minerals. The ore for treatment is a lead-zinc carbonate ore in a mixed siliceous-lime carbonate gangue. The association of […]

Silver Lead Zinc Ore Processing Method using Flotation

Silver Lead Zinc Ore Processing Method using Flotation - 911Metallurgist

Sulphide ore of lead and zinc containing considerable silver was submitted for testing with the purpose of determining a flowsheet for the production of separate lead and zinc concentrates for marketing at their respective smelters. It is necessary to recover as much silver as possible in the lead concentrate as a higher return for this […]

Sequential Copper–Lead–Zinc Flotation

Sequential Copper- Lead-Zinc Flotation Process Flowsheet

To improve the selectivity between copper and lead, a sequential copper-lead-zinc rougher circuit was tested. Each of the rougher circuits had a dedicated regrind and cleaner circuit. The advantages of the sequential circuits are that the levels of selectivity can be increased, particularly for copper and lead. With this process, copper was recovered first with MBS depression of lead, […]