Wooden Tank Capacity Tables – Diameter X Height

Source: This article is a reproduction of an excerpt of “In the Public Domain” documents held in 911Metallurgy Corp’s private library.
Guide to Flotation Cells in Mineral Processing

The flotation process and related flotation cells are widely used for treating metallic and nonmetallic ores and in addition, it is receiving an ever widening application in other industries. A greater tonnage of ore is treated by flotation than by any other single process. Practically all the metallic minerals are being recovered by the flotation process […]
Flash Flotation Cell

More profit can be earned by using the Flash Flotation Cell in the grinding Circuit. This machine has been designed especially for the recovery of floatable minerals at a coarse size as soon as the mineral is free; together with the finer sizes. Even though many ores require fine grinding to make the maximum recovery, […]
Jigging Separation Process Principle

The Mineral Jig is not just another gravity Separation Process. It is a highly efficient selective pulsator and concentrating machine which has the ability to treat an unclassified feed separating solids having only a slight differential in settling rates, with only a minimum addition of water. 1000s of these Mineral Jigging machines are now in operation on […]
Harz Jig Concentrators

Harz Type Jig The (Improved Harz Type) Jig is essentially a coarse – mineral Jig Concentrator embodying improvements on the Harz Jig and the Ellis Jig. It will handle successfully all types of ores which can be treated by gravity concentration with feed size ranging from ¼” to 1½”. These jigs are made in three sizes […]
Clarifying Filter

The Clarifying Filter is used to remove turbidity from practically any liquid. It can be used to remove either suspended solids or colloidal and dissolved solids, with the aid of an adsorbing agent. In certain cases a filter bed of porous material is used having decolorizing properties. In the majority of cases in metallurgical plants the filter […]
Rotary Dryer Design & Working Principle

For evaporating moisture from concentrates or other products from plant operations, Rotary Dryers are designed and constructed for high efficiency and economy in fuel consumption. Whenever possible to apply heat direct to the material to be dried, Rotary Dryers of the Direct Heating Design are used. If it is not possible to apply heat direct to […]
Small Jaw Crushers

We offer two types of forced feed and yet small jaw crushers: The Type “H” has cast steel or alloy iron frame, steel bumper with over-size roller eccentric bearings, bronze side bearings and manganese steel jaw and cheek plates. The Type “J” is made in two styles, one with bronze bearings and the other with anti-friction […]
Screw-Spiral Classifier: Select, Size & Install

The size of mechanical classifier required for a particular job depends on the following factors: Tons of dry solids to be overflowed per 24 hours. This is simply a predetermined tonnage. Mesh size at which separation is to be made. The mesh size is determined by laboratory tests or is already known from previous experience. […]
Hydroclassifier

Hydroclassifiers are solving the most difficult fine sizing and desliming problems by combining high metallurgical efficiency in a rugged, well- built machine to accurately fulfill the exacting conditions required. Accurate separations can now be made in the 100 mesh range and finer. This fine separation requires considerable classification area per ton as well as minimum […]