Elimination of Toxic Factors in Bio-oxidation of Sulfide Ores

Toxic substances in On solutions can retard biological leaching of copper sulfide dump ores. On solutions were analyzed for metals, organics, and chloride, and showed inhibitory concentrations of aluminum, manganese, and chloride. Inhibition of bacterial activity by the solid fraction of On solution, with and without the organic constituents, was evaluated. Materials and Methods The […]

Metals in Solutions – Dissolution Kinetic Modeling

A kinetic model for batch leaching of various metals with different lixiviants has been developed. Overall material balances for reactants and products at the solid/liquid interface were formulated with various types of heterogeneous reactions in place at the interface. The solutions to these mass balances have been identified analytically as well as numerically using a […]

How to Separate Heavy Rare Earth Elements

Potential increases in overall demand and purity requirements of rare-earth elements (REE) prompted the U.S. Bureau of Mines (USBM) to investigate new technology for separating these elements. REE, as defined by the USBM, include a group of 17 elements composed of Sc, Y, and the lanthanides. Although exact numbers are not available because of proprietary […]

ISL In-Situ Copper Leaching

In researching ways to improve the recovery of minerals from in situ leaching operations. Such operations are amenable to recovering low grade ore, reducing many of the typical mining operations cost, and presenting environmental benefits. Hydraulic properties and characteristics of copper ore are investigated to assess the impact of permeability on flow capacity during in-place, […]

Effect of Nonionic Surfactants on Chalcopyrite Leaching

Duncan, Trussell, and Walden reported the effect of nonionic surfactants on the Thiobacillus ferrooxidan leaching of chalcopyrite. The tests were conducted in 250-mL Erlenmeyer flasks containing minus 325 mesh chalcopyrite and a modified 9K medium at pH 2.5 and 35° C. The hypothesis tested in adding the surfactants was that the presence of a surfactant […]

Effect of Chalcopyrite Leaching Additives

Previous U.S. Bureau of Mines (USBM) research on the leaching of chalcopyrite with ferric sulfate [Fe2(SO4)3] demonstrates that surfactant additions enhance chalcopyrite (CuFeS2) leaching and that surfactant selection has a significant impact on the initial leaching rate. Additions of chloride ion (Cl-) are also known to enhance chalcopyrite leaching, although a review of the literature […]

Recovery of Mercury from Electrical Wastes

As part of its mission to reduce the environmental impact of minerals processing, the U.S. Bureau of Mines (USBM) investigated the characterization and treatment of Hg-contaminated wastes from an electrical-parts manufacturing plant. A literature search showed various hydrometallurgical methods for recovering Hg have been investigated on a laboratory scale, but there has never been a […]

HCl Hydrochloric Leaching of Manganese Silicate Ore

An estimated 17 million mt of manganese are contained in domestic manganese-bearing silicate resources, yet domestic production is insignificant compared with the quantity of manganese imported yearly into this country for consumption. The projected U.S. consumption of manganese in 1990 was expected to be about 680,400 mt with the majority of total demand being supplied […]

Recover Mercury from Concentrates by Chloride Leaching & Electrolysis

The Bureau of Mines and the Nevada Bureau of Mines have investigated hydrometallurgical methods for recovering mercury metal from sulfide concentrates. Most recently, Atkinson investigated the recovery of mercury from sulfide concentrates by a CuCl2 leaching- electrolysis technique. The concentrate used in the investigation was obtained from the McDermitt Mine, the major mercury producer in […]

Recover Cobalt in Copper Leach Solution by Ion Exchange

Significant amounts of cobalt, a strategic and critical metal, are present in some secondary sources such as spent copper leach solutions. The United States currently imports over 95 pct of its cobalt supply, much of it from Africa. Development of a process to recover cobalt from readily accessible spent copper leach solutions would help meet […]