Niton XRF Calibration Factors
On the Niton XRF, calibration factors are used to adjust for consistently high or consistently low readings from the XRF analyzer. They are calculated by graphing the data points created by plotting the percentage of each element as indicated by standard samples, against the percentage of each element as reported by the XRF analyzer. Then […]