Crushing, Screening & Conveying

Crushing, Screening & Conveying 2017-03-23T09:38:14+00:00
  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Crushing.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

flake generation problem in two roll smooth crusher (1 reply)

madineh
5 months ago
madineh 5 months ago

Hi, we use two roll crusher as secondary in pharaformaldehyd powder production plant (in closed loop) , but 30% of output material is in flake shape , roll dia :400 mm with : 350 mm input size: 10 mm output size : 2 mm , what can we do to decrease the flakes ?

Philip Stewart
5 months ago
Philip Stewart 5 months ago
1 like by David

Standard problem with roll crushers.  Run roll product through a. small hammer mill.

 