Dewatering: Thickening, Filtering, CCD, Water Treatment & Tailings Disposal

Dewatering: Thickening, Filtering, CCD, Water Treatment & Tailings Disposal

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Thickening, Filtering or Tailings and Water.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

INCO process recommendations (1 reply)

A
alenme
1 month ago
alenme 1 month ago

Hi

 

Does anyone have recommendations on the dissolved oxygen for the SO2/air process.

 

I could reach to 5-7 g/g SO2 to CN ratio and 8-10 pH ranges with 50 ppm of Cu but almost no recommendation is there in the literature regarding DO.

J
Jorge
13 hours ago
Jorge 13 hours ago

Regarding the Dissolved Oxygen (DO) in the reactors, it is important to maintain a low content, that usually should range from 2 to 5 mg/L. The equipment to determine the DO should be calibrated constantly to get the correct information.