Benchtop Ball Mill
US$12,000
This jar mill can be used as a Laboratory Bench-top Grinding Ball Mill or Rod Mill for the comminution of small samples, typically under 1 kg, for flotation tests or leach test.
- Ball: 7 5/8″ diameter x 6 3/4″ length (inner) = 5L
- Rod: 7 5/8″ diameter x 9 3/8″ length (inner) = 7L
- Mild steel construction
- Removable lid
- Bayonet-type lid closure
- Oversized rubber gasket
- Welded in lifter bars
- Machined rolling rings
Options
- Stainless steel construction
- Urethane or rubber-lined
- Rolls
- Grinding balls or rods
Categories: Ball Mills, Grinding Mills, Rod Mills
Description
2 roll x 24” long, 4″ diameter Laboratory Rolls Rubber covered steel rolls c/w shaft supported on self-aligning bearings, adjustable rolls, adjustable bottle retainers, 1/4 Hp motor/gear reducer drive with variable speed controller, OSHA type drive guards all mounted on common steel base. (support legs if required are extra).
Batch Rod Mill, mild steel construction complete with one (1) removable head with bayonet type lid closure, oversized rubber seal gasket, internal lifters and machined riding rings.
- 7-5/8” inside diameter x 9-3/4”
- 7-5/8” inside diameter x 6-3/4”
ADD-ON ROLLER STATION
Specifications
| Options:
|