1″ x 2″ Mini Rock Crusher

1″ x 2″ Mini Rock Crusher

US$1,200 $950

The 1″ X 2″ 911MPEJAC12 Small Rock Crusher is designed to finely crush rock and stone like aggregates or your favourite ore type (gold, silver, copper, etc.) from 3/4” (20mm) feed size down to a D50 – 50% passing 50 Mesh (300um).  canada manufacturer

This also correspond to a crushed products P80 size of 80% passing 1.5mm or 14 mesh.

This small jaw crusher and its miniature opening gape of 25 mm X 50 mm, can easily adjust by hand. The CSS, known as the closed-side-setting, can be choked down to effectively pulverize the rocks you feed in.
6 month warrantyWith a short throw at fast 500 RPM, this small rock breaker acts as a quasi-sample pulverizer without the dust of your typical cheap hammermill, chain beating, impact crusher amateur prospector often fall for and purchase online.

IN-STOCK

Description

mini jaw crusher (3)

Crusher Feed Hopper

The 911MPEJAC12 with a crushing capacity of 10 pounds (5 kg) per hours, ultra-portable (20 lbs.), and Small Rock Crusher is a Blake type crusher with a high-speed eccentric overhead. The product from this crusher is generally liberated enough and ready to pan or table for gravity gold separation.
When you buy this Small Rock Crusher, you also get: An operating manual, the pulley, pre-installed AR450 jaw plates. Without the 1 HP motor or mounting frame. This crusher can operate with gas/diesel engine as well as electric motor. Be sure to ration your speed/sheaves to have 500 RPM on the jaw and you are set to crush-those-rocks.

If you are looking for a ready-to-go prospector’s laboratory crusher, you can buy the mini laboratory version of the this rock crusher we also have for sale.

jaw_crusher


Rock Crusher Motor Pulley Size

Typical Motor for this Small Rock Crusher

jaw_crusher_motorhttp://www.harborfreight.com/engines-generators/electric-motors/1-hp-agricultural-farm-duty-motor-68288.html rock crusher motor belt

Example Rock Crusher Customer Installation

WE RECOMMEND INSTALLING A GUARD AROUND ALL MOVING PARTS
YOUR SAFETY, IS YOUR RESPONSIBILITY

mini-jaw-crusher-installation mini_homemade_stone_crusher
low_cost_jaw_crusher economic_jaw_crusher

SHIPPING & WARRANTY

mini-jaw-crusher

mini jaw crusher (1)

 

mini laboratory rock crusher (12)

 

mini rock crusher (4)

 

mini jaw crusher (12)


 

Rock Crusher Pulley Sizing

The crusher pulley diameter depends on your motor speed.

Use http://gadi.agric.za/software/renting/pulley_calc.php with crusher at 525 rpm.

Mini Crusher Operating Manual

To Be Read Prior to the Use of Mini Jaw Crusher

In order to maintain the long life and high performance standards your Crusher is designed for, it is essential to carefully observe and adhere to the following operating and maintenance instructions.123-portable-concrete-crusher-rental

*Once the Mini-Chipmunk Jaw Crusher is fully set up, run crusher empty for ½ hour for break in period*

HEALTH & SAFETY OPERATIONAL WARNINGS

  • EYE PROTECTION MUST BE WORN AT ALL TIMES while operating the rock crusher or while within 10ft of the machine. Pieces of stone can exit lid and enter the eyes causing injury or blindness.
  • HEARING PROTECTION MUST BE WORN AT ALL TIMES while operating the rock crusher. Prolonged exposure to noise levels above 85 decibels can damage hearing.
  • FOOT PROTECTION MUST BE WORN AT ALL TIMES while operating the rock crusher. Open toed footwear must never be worn around the machine. Stone can fall on operator causing injury.
  • LOOSE CLOTHING, LONG HAIR, DANGLING ACCESSORIES, JEWELLERY OR OTHER SIMILAR ITEMS THAT COULD CATCH MUST NOT BE WORN OR MUST BE PROPERLY SECURED WHILE OPERATING THE ROCK CRUSHER. Failure to do so can cause loose ends to get caught in moving parts resulting in injury or death.
  • DO NOT WEAR LOOSE FITTING GLOVES WHILE FEEDING ROCK CRUSHER. Only proper fitting gloves should be worn around rock crusher machine when handling sharp or rough materials. Do not wear loose fitting gloves, there is a risk of them get them caught in the machine resulting in injury.
  • AIR MASK MUST BE WORN WHILE OPERATING ROCK CRUSHER to prevent inhalation of dust and debris during operation. Prolonged inhalation of rock related dust can cause long term health damages to the lungs.

Mini Chipmunk Jaw Crusher INSTALLATION

Equipment Stand Installation:

For Jaw Crusher when supplied with 911Metallurgy Process Equipment Mini Chipmunk 1” X 2” Mounting stand:

  1. Before attaching 1”X 2” Jaw crusher assembly plate, ensure that stand site is secure. Stand should be set on flat even ground. Make sure each leg of stand is flush to ground surface and capable of supporting weight. Crusher is designed to operate on level surface, any slopes that cause crusher to sit at an angle will effect operating effectiveness. Warning: When Placing stand on soft materials, make sure all legs will remain equally supportive to avoid topple risk, which could result in damage to crusher, and operator.
  2. Carefully place 1”X 2” Jaw Crusher assembly plate carefully atop stand so the mini Jaw Crusher dispensary, and motor mount adjustments properly line up.188-gravel-crushers-for-sale
  3. Firmly Bolt down Jaw Crusher assembly to stand with all four corner mounting points.
  4. Check level and stand surface intermittently during operation to ensure stability and optimal performance.

For all other Stand mountings:

  1. Before attaching 1”X 2” Jaw crusher assembly plate, ensure that stand site is secure. Stand should be set on flat even ground. Ensure stand specifications are strong enough to support total weight of Crusher Mount. Make sure each leg of stand is flush to ground surface and capable of supporting weight. Crusher is designed to operate on level surface, any slopes that cause crusher to sit at an angle will effect operating effectiveness.Warning: When Placing stand on soft materials, make sure all legs will remain equally supportive to avoid topple risk, which could result in damage to crusher, and operator.
  2. Carefully place 1”X 2” Crusher mount atop stand. Ensure that nothing inhibits Crusher dispensary opening from underneath and that there is room for a bucket or collection hopper. Consider motor mount adjustment points and accessibility for future use.
  3. Firmly Bolt down Jaw crusher assembly with all four corner mounting points.
  4. Check level and stand surface intermittently during operation to ensure stability and optimal performance.

INSTRUCTIONS for Properly Feeding the Chipmunk Jaw Crusher 

*NEVER OPERATE ROCK CRUSHER WITHOUT SAFETY GUARDS PROPERLY IN PLACE OVER PULLEYS AND FLYWHEEL*

Once properly mounted to a stand, and with safety guards in place your Rock Crusher is ready to begin crushing rock. Adhering to the following steps will yield the best results:

  1. Before turning on Rock Crusher, make sure jaws are free of debris.
  2. Plate collecting bucket or trough underneath dispensary area of rock crusher to catch particles.
  3. When Rock Crusher is running, feed rocks with a maximum size of 3/4” into top of Crusher. Do not over feed Rock Crusher, for best results allow only half the jaw area to be filled with rock at one time. Do not fill crusher right up to top of the jaws, this puts too much pressure on jaws and can damage bearings.
  4. Speed and Particle size are a factor of how the lower jaw width is set. Read how to adjust dispensary particle size in order to make changes. Smaller Particle size the longer it will take the Jaw Crusher to work through rock, the Larger the particle size setting, the faster the jaw crusher can work through rock.

Other tips:

  • Rock Crusher should be used outside, or, in properly ventilated area.
  • Rock Crusher is designed to be used by adults. Parental supervision is needed for operators who are under the age of maturity.
  • Do not engage in horseplay while operating the rock crusher.
  • Always pay attention while operating the rock crusher.
  •  Do not operate rock crusher if you are sick, fatigued or is taking medications that cause drowsiness.
  • Only one person should feed the rock crusher at any one time.
  • Keep the floor around the rock crusher machine clean, dry and free from trip hazards. Do not allow chips to accumulate.
  • Users of rock crusher shall be aware of the location of first aid kits, fire exits, fire extinguishers, fire alarms, eye washes, deluge showers, emergency telephones and other safety related facilities.

JAW ADJUSTMENTS

*MAKE SURE JAW CRUSHER IS DISCONNECTED FROM POWER SOURCE BEFORE DOING ANY SERVICING OR ADJUSTMENTS*

Adjusting Jaws allows you change the ways the Crusher Jaws perform for different rocks and output requirements.

Adjusting Dispensary Particle Size can be done by adjusting the HEX nut on the back of the crusher between the crusher and engine.

To DECREASE particle size: Use ½” wrench to turn hex nut clockwise (Towards Pulley). Be aware of centric bearing position when measuring jaw opening.

Jaws should never run in contact with one another.

To INCREASE particle size: Use ½” wrench to turn hex nut counter clockwise (Towards FlyWheel). Be aware of centric bearing position when measuring jaw opening.