Geology & GeoMetallurgy

Geology & GeoMetallurgy

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Geology and Geometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

4
REPLIES
2156
VIEWS
Started by rios
I am starting a new gold mining project in Zimbabwe. I have contacted a Geologist and Geophysicist who did a Magnetic Survey on the target area. He also did a Resistivity and I.P. Survey. No other method was used and one has to dig 8 meters into muds...
r
Last replied to by rios
I  picked  rubble  from the  ground  and  took  100g  sample  for  fire  assay.  The result was 26g/ton.  That  is  quite  encouraging
1
REPLY
275
VIEWS
Started by ebnk15
Hypothetically, if I found sulfides while camping, would it be a waste of time looking downstream from these refractory gold ore locations for possible free gold? Or, would any free gold found have to come from an entirely different source? Does fre...
Last replied to by sediment-hosted-minerals
The short and simple answer is no. First of all, just because you find sulfides, there is no guarantee that gold is in the area. Often times the gold is disseminated within Pyrite crystals. It is so ...
2
REPLIES
440
VIEWS
Started by rcpa
Dear friends, I am interested in prospecting natural gold in  Brazil. I have seen many sites advertising gold detection devices, but I am very suspicious about the effectiveness of these equipments. Could anyone give me a hint how I should start my...
Last commented on by sediment-hosted-minerals
That's crazy timing! great list though. I think bottom line is that folks need to know that you cant just buy any metal detector and expect to find gold with it. Thank you for compiling the list.
2
REPLIES
978
VIEWS
Started by Ravele
I am conducting a research on recovering strategic elements from tailings. I am looking for a drilling company that will help with drilling the tailings dam for sample collection from the top to the bottom of the tailings dam, about 20-30 m deep.
S
Last replied to by SIMetallurgist
We had success with sonic drilling.
1
REPLY
987
VIEWS
Started by banoda
I have started gold mining in Ethiopia and looking for advice and information relating gold wash machine up to 8 ton per hour, and am newly born in conducting gold mining and have lease for land to explore and extract gold sand. I need your advice t...
Last replied to by sediment-hosted-minerals
Dear Banoda I just joined this site. Did you ever get your question answered? I can help.    
1
REPLY
899
VIEWS
Started by mkdevarajan
Does the industry accept resource model of Laterite Nickel deposits where the samples were assayed using Handheld XRF ?
J
Last replied to by Jorge
If the samples were pulverized and homogenized before using the handheld XRF analyzer, you could get good information. If the sample was not pulverized, only you will have information on the surface o...
2
REPLIES
855
VIEWS
Started by Millza79
Has anyone got any papers on the impact of ore variability (lithology, mineralogy, grade etc) on the financial performance of a process plant?
T
Last replied to by Todd H
My company has published a recent paper on geometallurgy here: https://www.convencionminera.com/perumin32/doc/conferencias/tecnologia/kgunesch-tt.pdf We do a lot of geometallurgy work and the paper ...
4
REPLIES
854
VIEWS
Started by ebnk15
Hi, Can someone provide me with any ideas, or help, on laying out a plan of operation for a BLM Prospecting Permit on National Forest Land in the Eastern Region? I am looking for gold, and have some ideas where I would like to search. Unfortunately,...
E
Last commented on by ebnk15
Yes, the land I am looking to prospect is acquired land, with a patchwork of private ownership. But, the Forest Ranger informed me that a BLM Prospecting Permit would be required. As a result, I am tr...
1
REPLY
774
VIEWS
Started by Leonita
Hi I just want to know how would I go about to determine if the sample we are sending after processing a half core is representative of the lot it is from? We start with a whole core that is halfed, sampled in 1m samples that is equal to 2/3kg that...
J
Last replied to by Jorge
If you have drill core samples, it is better to sent one half. You can consider two meters intervals. The lab will crush and split the samples following their procedures. At the end, the lab will give...
3
REPLIES
1245
VIEWS
Started by Bluegene66
Combination of high grade Zinc/Gold in a VMS system is very rare ie: 5m of 12% Zinc 14g/t Gold 1%Cu in a core sample. Can someone explain the structure and the significance of this unusual occurrence. Thanks.
8
Last commented on by
Do you have any gold or zinc in quantities you want to sell
2
REPLIES
1103
VIEWS
Started by aufinder
  Trying to Identify Ore pics attached close up and angles I believe this ore to be Cavarite ...(Krennerite or Sylvanite or Combo? or least gold Telluride Calaverite?  I have acid washed this Specimen once 2 weeks ago with muratic and it stayed ...
A
Last replied to by aufinder
Thanks I did a positive reaction with a small piece of the ore, and it was AU definately that it converted reacted into. I will have to extract the gold now, wow 66lbs at 40% gold is a lot of cash, ra...
9
REPLIES
1283
VIEWS
Started by montsep
I'm an environmental journalist and I'm preparing an article on photovoltaic cells. I would like to know the degree of exploitation of world quartz resources, and the current trend of this figure, given nowadays extraction rate. I'd like to know als...
R
Last replied to by Robert W Schafer
On a commercial scale metallurgical silicon metal is produced by the carbothermic reaction of silica (quartz) in an electric arc furnace using carbon electrodes where the temperature in the main react...
1
REPLY
1058
VIEWS
Started by NGVirginia
I have access to a Copper-Molybdenum tailings site with the following mineral content present (grams/ton): Bismuth - Bi (0.9), Selenium - Se (0.7), Tellurium - Te (0.4), Rhenium - Re (0.15), Gold - Au (0.015), and Silver - Ag (0.5). I am having diffi...
J
Last replied to by Jorge
Do you know the cooper grade?
2
REPLIES
985
VIEWS
Started by Nish
Hi guys, I've recently been given an opportunity to work on a geo metallurgy focused project, I however am a geologist and not very familiar with geo metallurgical processes. Could the metallurgists on here please advise on synthesis gold doped sy...
T
Last replied to by Todd H
Perhaps I dont fully understand - I dont think adding gold to pyrite is going to greatly enhance its flotability and certainly not going to enhance the project economics.  Pyrite is one of the easie...
2
REPLIES
1479
VIEWS
Started by lkperumal
Dear all,  I am searching about the magnetic properties of ferrosilicon ( 15% or 20% Si content). Anyone, please send me complete magnetic property details of FeSi with various composition. Thanks in advance
K
Last replied to by lkperumal
Thank you for your reply, Actually the question is about FeSi powder (in size range of microns). I have an idea to use this ferrosilicon powder to replace corbonyl iron powder in MR fluids. As it has...
0
REPLIES
966
VIEWS
Started by oluwatunmise
Hi everyone, Have been given an opportunity to talk on different approaches to gold exploration in basement terrain (i.e Geochemical, Geophysical, Geological, Mineralogical, etc). However, am a geologist but not well inclined to this approaches. plea...
2
REPLIES
1003
VIEWS
Started by Mattiel
Hello Everyone, we have recently acquired a claim with an old mine on it. We took some grab samples from inside the mine. We took samples from both the vein, and altered wall rock. We have done roughly 5 sets of testing with an average grade of ~15g/...
J
Last commented on by Jackievs
Apologies I was directing my question to Hamid...
1
REPLY
1119
VIEWS
Started by PJ
I work in a very heterogeneous, nuggety narrow vein gold deposit, and I am looking for a way to catch jumbo or longhole cuttings as a slurry before they land on the sill and become contaminated, and the gold separates. Has anyone here solved this iss...
S
Last replied to by Sylvain Tremblay
The solution would be very quick if your production drill was an In the Hole drill rig as you would be able to transform it, without a great investment into an RC drill rig and therefore catch your dr...
5
REPLIES
6506
VIEWS
Started by Charlie
Hello guys, does anybody know what variables are needed/ taken into account to establish an optimum ratio for ore blending? I'm blending two different Pb-Zn ROM samples (low and high grade).
O
Last replied to by OberstGruppen
About ore blending & stockpiles: Since the function of the stockpile is to act as an ore reservoir rather than as an ore processor, the action of forming a stockpile should have as little effect as ...
3
REPLIES
956
VIEWS
Started by louwrens
Hi all we have a mining operation, and our lab cannot explain the fire assay results provided, we did quite extensive test work on the ore and have received inconsistent results. Once the ore is delivered to our site the ore tests at 40-60 g AU per ...
F
Last replied to by Siddiquf
Representative sampling of broken ore is always problematical. Inconsistency in your case may simply be due to the sampler picking up the well mineralized pieces selectively in the first sampling.  
1
REPLY
940
VIEWS
Started by Moneer_Noor
we have several quality issues at magnesite mine (ultramafic alteratoin type). we are sampling 1 sample from blasthole material which depth in 4 meter for each hole to grade conrolling ROM. several quality issue is recorded. the mine material qualit...
Last replied to by Marshal Meru
I think it is also important to know the location of the sample. Blast hole sampling is the only one that gives you the location information. So I will keep this one for sure. I will try to reconcile ...
3
REPLIES
5437
VIEWS
Started by oro
Modern geophysical methods of mineral exploration are still too expensive for many small commercial scale placer miners, and seem to require a high level of learning and deployment.  I sometimes think / dream about a simple device that would measure...
J
Last replied to by oro
Thank you Rockdoc and Don for your responses. Basically I would like to buy a simple device (geophysical, not drill) to keep on hand, for simple estimates of depth to bedrock.  I see simple devices f...
1
REPLY
996
VIEWS
Started by Happiness
I need a scenarion where gravity method is deployed for inverstigating an ore body in contrast to the surrounding  
M
Last replied to by BAUD
Gravity separation is a concentration separation process in which minerals are separated from each other based on the difference of their specific gravity in a fluid medium. The applicability of grav...
1
REPLY
1110
VIEWS
Started by Witzcat
Dear experts, I would like to summarize all metals used for producing a car by calculating the mineral raw materials needed for each metal contained in a car. Of course I understand that each location and lagerstatte is different and there is not re...
Last replied to by David
This is a tough one. I did something similar just for the iPhone 6. https://www.usgs.gov/ was useful. I never did find what you are looking for exactly. I had to do math and plugin basic assumptions....
3
REPLIES
1845
VIEWS
Started by Nugget-hunter
identification of nugget of native metal found on the edge of granite country in northern Queensland Australia. SG of 5.4 and does not attract a magnet.    
T
Last replied to by Terrance
Process for extraction of platinum group metals from chromite-bearing ore US 4295881 A ABSTRACT A process for treating chromite-bearing ores to obtain useful mineral values, especially platinum ...
2
REPLIES
1102
VIEWS
Started by jlpalacios
Hi,   My name is José Luis, and I am doing my PhD about the assessment of mining/metallurgical processes by applying the Second Law of Thermodynamics. I am on the stage where I need to start to model a mining process. Would you mind telling me, w...
Last replied to by David
https://www.911metallurgist.com/blog/mineral-processing-extractive-metallurgy-methods https://www.911metallurgist.com/blog/mineral-processing-flowsheets
1
REPLY
980
VIEWS
Started by David
How can I know the price charges as well as the Recuperations of plant of a Silver Deposit in a Scoping Study?    
Last replied to by David
somebody hired you for this?
2
REPLIES
1526
VIEWS
Started by Simon-Flotation
During a recent visit to a copper mine in Chile, plant metallurgists mentioned they got colloidal silica in their ore, and it cause some process problems. I guess it is non-crystalline silica or amorphous silica, it has the same chemical structure wi...
b
Last replied to by Robert
There seems ample evidence that amorphous materials are present to surprisingly high extent in orebodies as mined as well as being created by reactions during processing. This includes siliceous, oxid...
3
REPLIES
1512
VIEWS
Started by Biglizer
Hello everyone I have some few questions to ask:  I encounter an outcrop of quartz vein larger more than 5 feet wide,first assay of a sample shows about 0.4ppm,i decided to do trenching and pit sampling...few samples by sorting show few gold by pa...
D
Last replied to by mkdevarajan
There are many places where isolated small quartz veins may give high grade gold mineralization which may support artisanal gold mining. But they may be far placed from each other that commercial mini...
4
REPLIES
2928
VIEWS
Started by Chifita
I recently came across such a mineralisation from an area with a lot of Hematite-Magnetite and just on the peripheral zones of the Lufilian Arc in Kasempa District of Zambia. I carried out a research which indicated that it was acicular malachite! ...
M
Last replied to by Mathias
Regarding the weird looking malachite, this mineral is readily soluble in weak acids. So it should reacht with hydrochloric acid. Did you test that? Regarding the other material. Frankly, I don't kno...
1
REPLY
1413
VIEWS
Started by Oberfuhrer
What is the maximum and minimum sampling interval that is suitable for drill cores from a first phase drilling in a porphyry Cu-Au deposit?
Last replied to by Paul Morrow
There is no simple answer to sample length, you need to consider geology, mineralisation, structural controls, drilling methods, mining methods, sample preparation techniques and ultimately is the cop...
1
REPLY
2095
VIEWS
Started by Kumar Choudhry
I am wondering about correct sampling procedure from a Full 30 tonnes Dump-truck of Iron ore with the top size of 30-35 Cm. would someone kindly help me to provide any literature.This sampling is required to provide the proper feed to the beneficiati...
Last replied to by Jean Rasczak
What you are suggesting is a very tough sampling problem at that top-size - much like the problem of draw-point sampling in underground cave mining methods.Unfortunately sampling theory would indicate...
3
REPLIES
1428
VIEWS
Started by Subhash-Kumar-Roy
Please could any one assist me in sampling procedure of Tailing dumps and low grade plies?
1
Last replied to by
It is essential to separate tailings, or other fine-grained material amenable to easy coring, from low grade stockpiles, or any other waste rock heap, which is particularly challenging to sample. It m...
4
REPLIES
2639
VIEWS
Started by Obersturmbann
I’m just wondering if anyone knows any good papers on the QA/QC of assay data.To date I have only been able to find one "Quality Control of Assay Data: A Review of Procedures for Measuring and Monitoring Precision and Accuracy" by Marat Abzalov, wh...
O
Last replied to by Obersturmbann
Thank you for the suggestions and help gentlemen, I'll follow them up in the next few days. If I come across any similar open source papers I will share them through this forum.
2
REPLIES
2354
VIEWS
Started by Helena Russell
Can anyone help me understand how to pin down possible reasons for getting only 37% of my original assays vs. pulp duplicates data plotting within 10% when I generate a HARD plot? I have over 400 pairs of data from three different labs. At each of th...
1
Last replied to by
Unless your gold is very fine then you are likely to get a fair bit of noise from the pulp duplicates. The first thing to check is how is the duplicate pulp collected - if is taken from jus the top of...