Impact of ore variability on the financial performance of a process plant? (2 replies)

Millza79
3 years ago
Millza79 3 years ago

Has anyone got any papers on the impact of ore variability (lithology, mineralogy, grade etc) on the financial performance of a process plant?

SmartDog
3 years ago
SmartDog 3 years ago

From a long time ago: Mining Methods Impact on Coal Preparation Plant Design
First International Mine Planning and Development Symposium, Beijing and Beidaihe, China, September 1980. 

 

T
Todd H
3 years ago
Todd H 3 years ago

My company has published a recent paper on geometallurgy here:

https://www.convencionminera.com/perumin32/doc/conferencias/tecnologia/kgunesch-tt.pdf

We do a lot of geometallurgy work and the paper above is part of a much larger ongoing study now in a feasibility for the project.  We built the mine plan and process recoveries from geometallurgical models that include recovery and ore hardness as the main outputs.

Regards

 

Todd Harvey - Global Resource Engineering http://www.global-resource-eng.com