  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Impact grinding flat gold / Garnet (1 reply and 2 comments)

akfury
2 months ago
akfury 2 months ago

Running flat gold & Garnet through impact mill / grinder.

Will the gold roll up into a ball somewhat?

I'm talking 20- concentrates.

SmartDog
1 month ago
SmartDog 1 month ago

No but it will get flatter, and probably break into smaller flakes.

akfury
1 month ago

Thanks for the reply. Dang. Not the answer I was looking for! Any other process you know of that will roll gold up?

SmartDog
1 month ago

Other than by hand, no

Please join and login to participate and leave a comment.

BUY Laboratory & Small Plant Process Equipment

We have all the laboratory and plant equipment you need to test or build/operate your plant.

ENTER our Mining Equipment' Store

We Sell EQUIPMENT for all types of Mineral Treatment PROCESSES and Laboratory Testing needs

Do you need METALLURGICAL TESTING of your ORE?

View the Services we Provide

911Metallurgist Mineral Processing & Process Development Laboratory

We have a metallurgical test for every possible mineral type and treatment.

Need ENGINEERING Services or Plant TROUBLESHOOTING?

We can IMPROVE ALL PLANTS / Mineral Processing Engineering & LABORATORY Ore Testing

911Metallurgy Engineering

Contact us for process engineering, metallurgical investigations, plant optimization, plant troubleshooting, needs. WE “FIX” METALLURGY.

I Need Consulting Engineering Help
I Need Ore Laboratory Testing