Grinding & Classification Circuits

Grinding & Classification Circuits 2017-04-04T06:57:16+00:00
  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Grinding.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Standards for design and sizing ball mill (2 replies and 3 comments)

msammet
2 years ago
msammet 2 years ago

Hi all,

Please can you help me to find standards for design and sizing ball mill (calculation of thickness of shell , Ø of shell , ... ) ?

best regards

David
2 years ago
David 2 years ago

Hello msammet, and welcome to 911Met Forums,

I do not have guidance on shell thickness.  Have you done a detailed read on http://www.911metallurgist.com/blog/ball-mill-design-power-example-calculation as it is a step-by-step example on Ball Mill design/sizing.

Including online calculators:

http://www.911metallurgist.com/blog/ball-mill-motorpower-sizing-calculation
http://www.911metallurgist.com/blog/how-to-size-a-ball-mill-design-calculator-formula
http://www.911metallurgist.com/blog/calculate-ball-mill-grinding-capacity

If you can be more specific in your question, I could maybe help you better.

David

msammet
2 years ago

Hello David ,
thank you David for your answer and I'm happy to join 911 Met Forums.
I am searching for both aspects, design and sizing ball mill (calculation of thickness of shell , Ø of shell , ... ) .
my request is there is a standards to determine :
- diameter and length of ball mill
- the thickness of the shell
- and other parameters needed for construction.

I hope that my request is clear .

Abdellatif

David
2 years ago
David 2 years ago

Hello Abdellatif,

I am certain there are standards with regards to thickness of the shells and the various parameters needed for construction of a ball mill.  I just do not know what they are.

What I know about diameter and length of ball mill is detailed in the example set by a ball mill manufacturer at http://www.911metallurgist.com/blog/ball-mill-design-power-example-calculation

For metallurgists, we are generally only considered with size the mill motor and shell lenght  + diameter itself as you can calculate at http://www.911metallurgist.com/blog/ball-mill-motorpower-sizing-calculation

http://www.911metallurgist.com/blog/how-to-size-a-ball-mill-design-calculator-formula

http://www.911metallurgist.com/blog/calculate-ball-mill-grinding-capacity

Stay present as others may have information I do not have.

David

David
2 years ago
msammet
2 years ago

thank you david
you are the best

Please join and login to participate and leave a comment.

BUY Laboratory & Small Plant Process Equipment

We have all the laboratory and plant equipment you need to test or build/operate your plant.

ENTER our Mining Equipment' Store

We Sell EQUIPMENT for all types of Mineral Treatment PROCESSES and Laboratory Testing needs

Have a Mineral Processing QUESTION?

Come in, ask your question

911Metallurgist Community Forums

Talk to other metallurgists and be helped.

Need ENGINEERING Services or Plant TROUBLESHOOTING?

We can IMPROVE ALL PLANTS / Mineral Processing Engineering & LABORATORY Ore Testing

911Metallurgy Engineering

Contact us for process engineering, metallurgical investigations, plant optimization, plant troubleshooting, needs. WE “FIX” METALLURGY.