Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Hydrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Ion exchange resin (1 reply)

P
max skinner
6 years ago
max skinner 6 years ago

I am looking for a ion exchange resin that will pull zinc out of a 15% sulfuric acid solution.

David
6 years ago
David 6 years ago

Hi Max,

my SX expert friend says "Why use a resin, conventional SX for zinc should work…high acid content though". PDF attached.