Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Hydrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Most Effective Solvent Extraction Method (1 reply and 1 comment)

B
LenjeLeonheart
7 years ago
LenjeLeonheart 7 years ago

I was wondering what solvent extraction method you all would believe to be the most cost effective for a small scale refining op, and the steps you would recommend taking for said method? I'm starting from ore.

Thank you for your time,

Bradford

(unknown)
7 years ago
(unknown) 7 years ago

I am flummoxed by your question……”starting with ore”, refining? Solvent extraction method?

Solvent extraction is a method or process for concentrating and “purifying” leach solutions to upgrade desired metal concentration prior to subsequent plating by electrolysis (electro-winning) which requires no further refining. Occasionally solvent extraction is used prior to a precipitation process.

B
LenjeLeonheart
7 years ago

I'm trying to use a precipitation process to get the precious metals out of the ore, as opposed to just crushed-
panning or smelting it