Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Hydrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Sulfide gold ore treatment by roasting (1 reply)

C
canerdogan
6 days ago
canerdogan 6 days ago

Hi,

How to i know the ore is calcined or not at the roasting stage before heap leach process. 

J
Jorge
4 days ago
Jorge 4 days ago

Roasting is considered a pre-treatment before Carbon-in-Leach Process to treat a refractory gold ore. It is necessary to perform a testing program to determine the effect of particle size (e.g. 70, 50, 40, 30 um K80), temperature (e.g. 500, 600, 700 oC) and residence time (e.g. 1. 2, 3 h) on gold leaching. Gold dissolution is evaluated performing bottle roll tests. For example, If the gold extraction is as high as 90%, the roasting parameters are correct.