Remove Trash from Flotation Circuit via Screen-Box in Grinding Circuit

An on-stream analyzer and small regrind cyclones (their small 1/2″ Apexes) were being plugged by trash coming from the underground mine in the form of wood and plastic. A simple solution was to install a homemade screen box on the cyclone overflow prior to feeding flotation. The operator cleans it daily, thanks to the overhead […]