SX Solvent Extraction Equipment – Process Function
Mixer Settler The Mixer-Settlers are of the pump-mixer type in which the Mixer Impellers, in addition to mixing the process liquors, also provide the pumping head necessary to transfer them between stages. The variable speed Impellers can be used either with, or without, spoiler blades, the design of which is such that when fitted the […]
Segregation Process of Mixed Sulphide Copper Ore

Sulphide copper ores are normally concentrated by flotation while the oxide ores undergo hydrometallurgical treatments. The mixed sulphide-oxide copper ores may be processed by combined methods such as flotation followed by leaching and precipitation of the oxidized portion, or vice-versa. Also a Leach-Precipitation-Float Process (LPF Process) has been successfully applied. However, when oxide or mixed […]